石英仿石砖生产中会存在的问题
石英仿石砖质地坚硬,经得起风雨,现在已经在各个地方使用了,随着技术的不断发展,创意瓷砖来迎合大家的家居装修理念,那大家知道山东石英仿石砖生产过程中会出现哪些问题吗?下面厂家介绍一下:
Quartz imitation stone bricks have a hard texture and can withstand wind and rain. They have been used in various places now. With the continuous development of technology, creative ceramic tiles have catered to everyone's home decoration concepts. Do you know what problems may arise during the production process of quartz imitation stone bricks in Shandong? The following is an introduction from the manufacturer:
1、破碎:是指将石英仿石砖破碎成一定比例的颗粒,但破碎颗粒的大小和比例会影响其透水性、表面效应、强度、半成品尺寸和烧成温度,颗粒越粗,透水性越好,但坯体强度会降低,表面效果粗糙,尺寸增大,烧成温度升高。
1. Crushing: refers to breaking quartz imitation stone bricks into particles of a certain proportion, but the size and proportion of the broken particles will affect their water permeability, surface effect, strength, semi-finished product size, and firing temperature. The thicker the particles, the better their water permeability, but the strength of the body will decrease, the surface effect is coarse, the size increases, and the firing temperature increases.
2、在混合搅拌过程中,加入一定量的熔剂和粘结剂,提高生坯的强度和球团之间的附着力,如果不加就不能成型,或者强度不够,半成品损耗大,成品石英仿石砖有很多裂纹。
2. During the mixing and stirring process, a certain amount of flux and adhesive is added to improve the strength of the green body and the adhesion between the pellets. If it is not added, it cannot be formed, or the strength is insufficient, resulting in large loss of semi-finished products, and many cracks in the finished quartz imitation stone brick.
3、如果成形压力机是自动压力机,它需要一个辅助分配系统,石英仿石砖通常由织物和基材组成,织物与基材的比例约为1:6,对于仿砖的成型,在降低设备投资、设备维护成本和使用廉价劳动力的同时,很多企业会采用摩擦压砖机或振动压砖机来满足工艺要求。
3. If the forming press is an automatic press, it requires an auxiliary distribution system. Quartz imitation stone bricks are usually composed of fabric and substrate, with a ratio of about 1:6. For the formation of imitation bricks, while reducing equipment investment, equipment maintenance costs, and using cheap labor, many enterprises will use friction or vibration presses to meet process requirements.
4、窑烧通常用于烧制石英仿石砖,其厚度约为60毫米,烧制时间约为20小时,同时,棚车大约有八层,烧成温度为1200-1250摄氏度。
4. Kiln firing is commonly used to fire quartz imitation stone bricks, which have a thickness of about 60 millimeters and a firing time of about 20 hours. At the same time, the box car has about eight layers and a firing temperature of 1200-1250 degrees Celsius.
以上就是石英仿石砖生产过程中会出现的问题,通过这些描述,相信大家有了更深的了解,如果在使用中遇到问题,可以多和厂家//www.quanyouyou.com沟通。
The above are the problems that may occur during the production of quartz imitation stone bricks. Through these descriptions, I believe you have a deeper understanding. If you encounter problems during use, you can contact the manufacturer more often //www.quanyouyou.com communicate.